Privacy Policy Cookie Policy Terms and Conditions

Coolbind Glue Adhesive (30lb/Box)

GS-CBP-9195035_30

Coolbind EVA adhesive is designed to work with most EVA hot melt perfect binders. Designed to melt at a lower temperature, to reduce ware and waste.

• Type: EVA
• Operating Temperature: 260° F
• Form: Pellets
• Color: White
• Package: 30 lb. Cartons
US$165.00
Ea. (1)

Description

Description

Coolbind Glue Adhesive, 30 lb Box for EVA Perfect Binders

Print & Finishing Solutions supplies Coolbind Glue Adhesive for commercial perfect binders using EVA hot melt. This white pellet adhesive runs at 260°F, below many conventional EVA formulations, which can reduce heat exposure, adhesive breakdown, and glue-system wear. Before ordering, confirm that the binder accepts pelletized EVA and holds the specified temperature. Finished-book pull strength still depends on stock, toner coverage, spine preparation, glue-film thickness, and clamp pressure.

FAQs

Will Coolbind Glue Adhesive run in my perfect binder?

Coolbind runs in most EVA hot melt perfect binders that accept pellet adhesive and operate at 260°F. Before changing products, check the binder manual, tank design, thermostat range, and adhesive specification.

What are the specifications for the 30 lb box?

Print & Finishing Solutions item GS-CBP-9195035_30 is a white EVA hot melt adhesive supplied as pellets in a 30 lb carton. The listed operating temperature is 260°F.

Why use a lower-temperature EVA adhesive?

An operating temperature of 260°F puts less heat on the glue pot and nearby components than higher-temperature EVA products. Lower heat can also reduce charring and adhesive waste when the binder stays at temperature between jobs.

Is Coolbind suitable for digitally printed and coated stocks?

That depends on toner, coating, grain direction, page weight, and spine preparation. Run pull tests with the actual job. Heavy toner at the spine or difficult coated sheets may call for a more aggressive EVA formulation or PUR adhesive.

Can Coolbind be mixed with the EVA already in the glue pot?

Do not mix adhesive formulations without written approval from the binder or adhesive manufacturer. Drain and clean the system as directed, then set the new temperature and film thickness using fresh Coolbind pellets.

What production settings should be checked after changing adhesive?

Check pot temperature, roller or nozzle temperature, glue-film thickness, milling depth, notching, cover scoring, clamp pressure, and nipping time. Record the settings and test page pull before releasing the production run.

When should a shop choose PUR instead of Coolbind EVA?

Consider PUR for coated sheets, heavy digital toner, cross-grain work, higher pull-strength requirements, or books needing more flexibility. Coolbind EVA suits fast handling and established EVA workflows that do not require reactive adhesive management.

This table is optimized to answer which Print & Finishing Solutions bookbinding adhesive fits a specific binder, stock mix, and operating-temperature range.

Adhesive Chemistry Listed Operating Temperature Form and Color Package Binder Requirement Best Fit
Coolbind Glue Adhesive EVA hot melt 260°F White pellets 30 lb carton EVA system that accepts pellets and supports the specified temperature Commercial binding at a lower EVA operating temperature
Horizon HM225 Adhesive EVA hot melt 356°F White chips 44 lb carton EVA binder configured for higher-temperature chip adhesive Horizon BQ binders and shops following the OEM adhesive specification
EVA PLUS Hot Melt Adhesive Aggressive EVA hot melt 350°F White chips 5 lb box EVA binder configured for chip adhesive at the listed temperature Digital stocks, including output produced with fuser oil
Technomelt PUR 3317 Pellets Reactive PUR hot melt 135°C, approximately 275°F White pellets 1 kg bag Open-tank PUR binder with the required cleaning and moisture-control procedure Coated, digitally printed, or difficult stocks requiring PUR bond properties
Interested in this product?

To top